Hastelloy B
Komposisi Kimia
Paduan | unsur | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Paduan B2 | Min | 26.0 | |||||||||
Max | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Kasaimbangan | 1.0 | 30.0 | 2.0 | 1.0 |
Sipat mékanis
Status Aolly | Kakuatan regangan Rm Mpa Min | kakuatan ngahasilkeun RP 0. 2 Mpa Min | Elongation A 5% Min |
Solusi | 745 | 325 | 40 |
Pasipatan fisik
Kapadetan g / cm3 | Titik lebur ℃ |
9.2 | 1330-1380 |
Standar
Rod, Bar, Kawat jeung Forging Stock- ASTM B 335 (Rod, Bar), ASTM B 564 (Forging), ASTM B 366 (Pasang)
Piring, Lambaran sareng Strip- ASTM B 333
Pipa jeung Tube- ASTM B 622(Seamless) ASTM B 619/B626(Tabung Dilas)
Ciri hastelloy B2
● lalawanan hébat kana stress korosi cracking na pitting
● Résistansi anu signifikan pikeun ngirangan kaayaan sapertos hidrogén klorida, asam sulfat, asétat sareng fosfat
● Résistansi kana asam hidroklorat dina sagala konsentrasi sareng suhu
● saméméhna: INCONEL® alloy C-276 UNS N10276 / W.Nr. 2.4819
● Salajengna: HASTELLOY B-3 UNS N10675/W.Nr.2.4600
Tim kami sanés ngan ukur sakelompok profésional anu gaduh pangalaman mangtaun-taun dina perdagangan internasional. Kami inovator, terus-terusan narékahan pikeun ngadorong wates naon anu mungkin. Pamakéan produk mutakhir sapertos Hastelloy B2 UNS N10665 W.NR.2.4617 ngagambarkeun komitmen urang pikeun tetep payuneun kompetisi sareng nyayogikeun jasa anu pangsaéna pikeun para nasabah. Gabung kami dina usaha kami pikeun ngadamel dampak anu langgeng dina industri sareng ngalaman heula kakuatan pamikiran inovatif.