Biphase Stainless Steel

  • SUPER DUPLEX S32760 / F55 / 1.4501

    Super Duplex S32760/ F55, Super Duplex Alloy UNS S32760 (F55 / 1.4501) gaduh résistansi Pitting sareng Crevice Corrosion dina cai laut dina suhu anu luhur, disayogikeun ku PREN 40<( Pitting Resistance Eqv). Résistansi anu saé pikeun SCC (Stress Corrosion Cracking) dina lingkungan Asam sareng Klorida.

  • Super dupleks 2507 kualitas luhur

    ● UNS S32750, F53
    ● ASTM A 240, A790, A815, A182, A 276, A 476, A789
    ● EN 1.4410
    ● Ngaran umum lianna SAF 2507®

  • Biphase Stainless Steel

    Alloy Suhu Tinggi Komposisi kimia Kelas C Si Mn SP Cr Ni Mo Cu NW lian teu langkung ageung tibatan F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08~0.2 - - F53 0.0.2 - - F53 0.0.8 ~ 26 6 ~8 3~5 ≤0.5 0.24~0.32 — - F55 0.03 1 1 0.01 0.03 24~26 6~8 3~4 0.5~1 0.2~0.3 0.2~0.3 0.3 0.5 .035 23~28 3~6 1 ~3 - - - - A4 ...